RE: First 30 minites with the LW sit and climb
GMMAT, they are cast aluminum correct?
I am a Corporate Process/Tooling Engineer for a fairly large Aluminum die caster...upon my review(which would be majorly heightened than the average joe)of the quality I was shocked!!! These are finished insome form of a powder coat, which gives it a nice finish....BUT....the flash (no noto 90% of out customers, 100% if there is ANY and I mean any cosmetic or handling requirement) off of the ejector pins and parting line was still present, the gate and overflow vestige was rediculous as was trim shear....there was also RAW aluminum showing = huge customer reject problem if caught to 99.9% of products....the defects ARE visual to the average joe and that is my complaint!!! Does that help with my JUNK comment????