Semi - go on. You're full of it. You're always fluxing around!
bronko22000 is offline  
Reply
Old 02-15-2012 | 08:34 PM
  #12  
Semisane's Avatar
Boone & Crockett
 
Joined: Apr 2007
Posts: 10,918
Likes: 1
From: River Ridge, LA (Suburb of New Orleans)
Default

Not so much anymore Bronko. I was a dedicated fluxer in my younger days though.
Semisane is offline  
Reply
Old 02-18-2012 | 12:52 PM
  #13  
HuntAway's Avatar
Nontypical Buck
 
Joined: Mar 2005
Posts: 1,392
Likes: 0
From: Renfrew County, Ontario, Canada
Default

You two fluxers. What is the purpose/ what is flux?

HA
HuntAway is offline  
Reply
Old 02-18-2012 | 02:09 PM
  #14  
corey012778's Avatar
Nontypical Buck
 
Joined: Aug 2007
Posts: 3,713
Likes: 0
From: Staunton,Va
Default

Originally Posted by HuntAway
You two fluxers. What is the purpose/ what is flux?

HA
fluxing is the act of adding something to melted metals to draw out impurities.

ie: beeswax to melted lead
corey012778 is offline  
Reply

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are Off



Contact Us - Archive - Advertising - Cookie Policy - Privacy Statement - Terms of Service -

Copyright © 2026 MH Sub I, LLC dba Internet Brands. All rights reserved. Use of this site indicates your consent to the Terms of Use.